| 3541 |
National Test House (ER), Kolkata
| IS 1848 : Part 2 (2018) - Writing and printing papers - Specification: Part 2 air mail/manifold, cartridge drawing and cartridge white, duplicating absorbent and duplicating semi - Absorbent and poster machine glazed types (Fifth Revision) |
Writing and printing papers - Specification: Part 2 air mail/manifold, cartridge drawing and cartridge white, duplicating absorbent and duplicating semi - Absorbent and poster machine glazed types (Fifth Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 4.2 (Substance (Grammage),) |
1000.0 |
|
| 4.3 (Thickness) |
1000.0 |
|
| 4.5 (pH (Hot Extract)) |
1000.0 |
|
| 4.6 (Tensile Index) |
1500.0 |
|
| 4.6 (Brightness) |
2000.0 |
|
| 4.6 (Opacity) |
2000.0 |
|
| 4.6 (One Minute Cobb) |
2000.0 |
|
| 4.6 (Double Fold) |
1500.0 |
|
| 4.6 (Gloss) |
1500.0 |
|
| 4.6 (Wax Pick) |
2000.0 |
|
| 4.6 ( Smoothness Bendsten) |
2000.0 |
|
| 4.6 (Tear Index) |
2000.0 |
|
|
| 3542 |
National Test House (ER), Kolkata
| IS 1848 : Part 1 (2018) - Writing and printing papers - Specification: Part 1 account book, azure lead, bond, cream laid and cream wove/printing white/printing coloured/printing offset, printing maplitho, printing white super calendered and typewriting types (Fifth Revision) |
Writing and printing papers - Specification: Part 1 account book, azure lead, bond, cream laid and cream wove/printing white/printing coloured/printing offset, printing maplitho, printing white super calendered and typewriting types (Fifth Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 4.2 (Substance (Grammage), g/sq.m) |
1000.0 |
|
| 4.3 (Thickness) |
1000.0 |
|
| 4.5 (pH (Hot Extract)) |
1000.0 |
|
| 4.6 (i) b (Tensile Index (MD)) |
1000.0 |
|
| 4.6 (Brightness, %) |
2000.0 |
|
| 4.6 (Opacity, %) |
2000.0 |
|
| 4.6 (One Minute Cobb) |
1000.0 |
|
| 4.6 (Folding Endurance) |
1500.0 |
|
| 4.6 (Wax Pick) |
1500.0 |
|
| 4.6 (vii) (Wax Pick) |
2000.0 |
|
| 4.6(viii) (Smoothness Bendsten) |
2000.0 |
|
| 4.6(ix) b (Tear Index (CD)) |
1000.0 |
|
| 4.4 (Sizes and tolerance on size) |
1000.0 |
|
| 4.6 (i) a (Tensile Index (CD)) |
1000.0 |
|
| 4.6 (i) b (Tensile Index (MD)) |
1000.0 |
|
| 4.6 (ix) a (Tear index(MD)) |
1000.0 |
|
| 4.6(ix) b (Tear Index (CD)) |
1000.0 |
|
| 4.6 (v) b (Double fold (CD)) |
750.0 |
|
| 4.6 (v) a (Double Fold (MD)) |
750.0 |
|
| 4.6 (viii)b (Smoothness Bendsten (Wire Side), ml/min) |
1000.0 |
|
| 4.6 (viii)a (Smoothness Bendsten (Top Side), ml/min) |
1000.0 |
|
| Firm's request (Mechanical Pulp Content(%)) |
- |
|
| Firm's request (Free From Specks) |
1000.0 |
|
| Firm's Requirement (Surface Sizing) |
1000.0 |
|
|
| 3543 |
National Test House (ER), Kolkata
| IS 1084 (2005) - Textiles – Manila ropes – Specification (fifth revision) |
Textiles – Manila ropes – Specification (fifth revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 6.1 (Identification of Fibre) |
2000.0 |
|
| 6.5 (Oil Content) |
2000.0 |
|
| 6.6 (Zn) |
1000.0 |
|
| 8.2 (Pitch) |
500.0 |
|
| 8.4 (Diameter) |
500.0 |
|
| 8.5.3 (Linear Density) |
1000.0 |
|
| 8.5.5.6 (Breaking Strength, KN) |
3000.0 |
|
| 6.4 (Lay of Rope) |
500.0 |
|
| 6.3 (Lay of Strand) |
500.0 |
|
| 6.5 (Number of Yarn per Strand) |
500.0 |
|
| 6.4 (No. of Strands) |
500.0 |
|
|
| 3544 |
National Test House (ER), Kolkata
| IS 1891 : Part 1 & ISO 340 (1994 & 2013) - Conveyor and elevator textile belting - Specification: Part 1 general purpose belting (Fourth Revision) |
Conveyor and elevator textile belting - Specification: Part 1 general purpose belting (Fourth Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 5.1 (Construction) |
1000.0 |
|
| 8.1.1 (Thickness of Cover, mm.) |
1000.0 |
|
| 13.2 (Width) |
1000.0 |
|
| 7.4 (Tensile Strength of cover rubber) |
2000.0 |
|
| 7.4 (Elongation of cover rubber) |
1000.0 |
|
| 7.3 (Percent Variation in Tensile Strength after ageing at 70(+/-) 1 deg C for 72 hrs , %) |
3000.0 |
|
| 7.3 (Percent Variation in Elongation after ageing at 70(+/-) 1 deg C for 72 hrs , %.) |
2000.0 |
|
| 7.4 (Abrasion Loss) |
3000.0 |
|
| 14.1 (Full Thickness Breaking Strength) |
5000.0 |
|
| 14.2.1 (Elongation at reference load, percent) |
1000.0 |
|
| 14.2.2 (Elongation at break , percent) |
1000.0 |
|
| 15 (Adhesion Strength between plies) |
3000.0 |
|
| 15 (Adhesion beween cover & carcass) |
2000.0 |
|
| Firm's request. (Hardness(Shore A).) |
1000.0 |
|
| 4.0 (Flame Test) |
4000.0 |
|
| Firm's request. (Electrical Resistance) |
5000.0 |
|
| Firm's request. (Angular Tear Strength) |
2000.0 |
|
| Firm's request. (Hardness(Shore A).) |
1000.0 |
|
|
| 3545 |
National Test House (SR), Chennai
| IS 2185 : Part 1 (2005) - Concrete masonry units - Specification: Part 1 hollow and solid concrete blocks (Third Revision) |
Concrete masonry units - Specification: Part 1 hollow and solid concrete blocks (Third Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 9.5 (Water Absorption-Annex E of -IS 2185 : Part 1) |
1000.0 |
|
| 9.4 & Table2 (Compressive Strength-Annex D of -IS 2185 : Part 1) |
4000.0 |
|
| 9.3 & 5 (Block Density-Annex C of -IS 2185 : Part 1) |
1000.0 |
|
| 9.2, 4.2.3 & Table 1 (Dimensions-Annex B of -IS 2185 : Part 1) |
500.0 |
|
| 9.1 (General -IS 2185 : Part 1) |
500.0 |
|
|
| 3546 |
National Test House (SR), Chennai
| IS 2185 : Part 3 (1984) - Concrete Masonry Units Part 3 Autoclaved Cellular Aerated Concrete Blocks |
Concrete Masonry Units Part 3 Autoclaved Cellular Aerated Concrete Blocks |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 8.6 (Drying Shrinkage, in %) |
1000.0 |
|
| 8.4 (Compressive Strength, in N/mm²) |
12000.0 |
|
| 8.3 (Block Density, kg/m³) |
1000.0 |
|
| 8.2 (Dimensions (Length, width and thickness)) |
3000.0 |
|
| 8.1 (General ) |
500.0 |
|
| 8.4 (*Compressive strength (Average of 3 blocks),N/mm2) |
3000.0 |
|
| 5 (Moisture Content (as received condition), on the lines of IS 6441, %) |
1000.0 |
|
| custom (Water absorption (Annex E of IS 2185(Part 1):2005)) |
1000.0 |
|
| custom (Efflorescence -on the lines of IS 3495(3)) |
1000.0 |
|
|
| 3547 |
National Test House (SR), Chennai
| IS 1079 (2017) - Hot rolled carbon steel sheet, plate and strip - Specification (Seventh Revision) |
Hot rolled carbon steel sheet, plate and strip - Specification (Seventh Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 10 (Cupping Test) |
2000.0 |
|
| 9 (Bend Test) |
1000.0 |
|
| 8.3 (Elongation) |
1000.0 |
|
| 8.3 (Tensile Strength for Designation Ordinary, Commercial and General purpose.) |
2000.0 |
|
| 8.3 (0.2 Proof Stress / Yield Stress (Drawing quality)) |
1000.0 |
|
| 13 (Dimensions) |
1000.0 |
|
|
| 3548 |
National Test House (SR), Chennai
| IS 737 (2008) - Wrought aluminium and aluminium alloy sheet and strip for general engineering purposes - Specification (Fourth Revision) |
Wrought aluminium and aluminium alloy sheet and strip for general engineering purposes - Specification (Fourth Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 7.2 (Bend Test) |
1000.0 |
|
| 7.1 (% Elongation at 50 mm gauge length) |
500.0 |
|
| 7.1 (0.2% Proof Stress) |
1000.0 |
|
| 7.1 (Tensile Strength) |
1000.0 |
|
| 9 (Dimensions) |
1000.0 |
|
| 6 (Titanium) |
1000.0 |
|
| 6 (Silicon) |
1000.0 |
|
| 6 (Manganese) |
1000.0 |
|
| 6 (Chromium) |
1000.0 |
|
| 6 (Magnesium) |
1000.0 |
|
| 6 (Iron) |
1000.0 |
|
| 6 (Copper) |
1000.0 |
|
| 6 (Zinc) |
1000.0 |
|
| 6 (Aluminium) |
1000.0 |
|
|
| 3549 |
National Test House (SR), Chennai
| IS 15622 (2017) - Pressed Ceramic Tiles - Specification (First Revision) |
Pressed Ceramic Tiles - Specification (First Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 6, Tables 8 and 9, Sl No (ii), (q) (Bulk Density-IS13630 (Part 2):2019) |
1000.0 |
|
| 6, Tables 5 to 9, Sl No (ii), (k) (Impact resistance-Coefficient of Restitution-IS13630 (Part 14):2019) |
1000.0 |
|
| 6, Tables 5 to 9, Sl No (ii), (j) (Crazing Resistance- IS13630 (Part 9):2019) |
1500.0 |
|
| 6, Tables 5 to 9, Sl No (ii), (g) (Coefficient of Linear thermal expansion from ambient temperature to 100° C(K raise to -1)-IS 13630 (Part 4):2019) |
1000.0 |
|
| 6, Tables 5 to 9, Sl No (ii), (e) (Scratch Hardness of surface (Mohs' Scale)-IS13630 (Part 13):2019) |
2000.0 |
|
| 6, Tables 5 to 9, Sl No (ii), (c) (Breaking of strength in N- IS13630 (Part 6):2019) |
2000.0 |
|
| 6, Tables 5 to 9, Sl No (ii), (b) (Modulus of rupture in N/mm²- IS13630 (Part6):2019) |
2000.0 |
|
| 6, Tables 5 to 9, Sl No (ii), (a) (Water Absorption-IS13630 (Part 2):2019) |
1000.0 |
|
| 6, Tables 5 to 9, Sl No (i), (e-1,2,3) (Surface Flatness-Maximum deviation in percent from flatness-(Centre curvature, Edge curvature & warpage) -IS: 13630 (Part1):2019) |
500.0 |
|
| 6, Tables 5 to 9, Sl No (i), (c) (Straightness of sides(Facial sides)Maximum deviation in percent to corresponding work size- IS13630 (Part1):2019) |
500.0 |
|
| 6, Tables 5 to 9, Sl No (i), (d) (Rectangularity-Maximum deviation in percent to corresponding work size-IS: 13630 (Part1):2019) |
500.0 |
|
| 6, Tables 5 to 9, Sl No (i), (b) (Dimension-Thickness-Deviation in percent from work size -IS: 13630 (Part1):2019) |
1000.0 |
|
| 6, Tables 5 to 9, Sl No (i), (a) (Dimensions-Width -IS:13630 (Part1):2019) |
1000.0 |
|
| 6, Tables 5 to 9, Sl No (i), (a) (Dimensions-Length-IS13630 (Part1):2019) |
1000.0 |
|
| 6, Tables 5 to 9, Sl No (i), (f) (Surface Quality-IS13630 (Part1):2019) |
500.0 |
|
| 6, Tables 5 to 9, Sl No (iii), (c) (Resistance to acid and alkalies (with exception of hydrofloric acid and its compounds-IS 13630(8)/(7):2019) |
1000.0 |
|
| 6, Tables 5 to 9, Sl No (iii), (b) (Resistance to household chemicals swimming pools, and water cleansers except to cleansing agents containing hydrofluoric acid and its compounds IS 13630(8)/(7):2019) |
1000.0 |
|
| 6, Tables 5 to 9, Sl No (iii), (a) (Resistance to staining IS 13630(8)/(7):2019) |
1000.0 |
|
|
| 3550 |
National Test House (NR), Ghaziabad
| BSEN 13348 (2016) - Copper and Copper Alloy - Seamless Round Copper Tube for Medical Gases or vacuum |
Copper and Copper Alloy - Seamless Round Copper Tube for Medical Gases or vacuum |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 6.2 (Tensile Strength) |
2000.0 |
|
| 6.1 (Cu + Ag) |
4000.0 |
|
| 6.1 (Phosphorus (% by mass)) |
1000.0 |
|
| 6.2 (Elongation) |
1000.0 |
|
| 6.2 (Hardness) |
2000.0 |
|
|
| 3551 |
National Test House (WR), Mumbai
| IS 1786 (2008) - High strength deformed steel bars and wires for concretere inforcement - Specification (Fourth Revision) |
High strength deformed steel bars and wires for concretere inforcement - Specification (Fourth Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 4.2 (18) (Chemical Composition with micro alloying elements, % by mass.) |
4000.0 |
|
| 4.2 (17) (Chemical Composition without micro alloying elements, % by mass.) |
2000.0 |
|
| 7.2 (Mass per metre run, kg/m - IS 1786: 2008) |
1000.0 |
|
| 9.2 (4) (Tensile Strength (up to 12 mm), N/mm² - IS 1608 (Part 1): 2022.) |
- |
|
| 9.2 (5) (Tensile Strength (16 to 28 mm), N/mm² - IS 1608 (Part 1): 2022.) |
1000.0 |
|
| 9.2 (6) (Tensile Strength (32 to 40 mm), N/mm² - IS 1608 (Part 1): 2022.) |
1500.0 |
|
| 9.2 (Yield Stress/ 0.2 % Proof Stress. N/mm² -- IS 1608 (Part 1): 2022.) |
1000.0 |
|
| 9.2 (1) (TS/ YS Ratio - (IS 1786: 2008/ IS 1608 (Part 1): 2022).) |
- |
|
| 9.3 (Bend test - IS 1599: 2023.) |
1000.0 |
|
| 9.4 (Rebend test (0 - 28 mm) - IS 1786: 2008) |
1000.0 |
|
| 9.4 (1) (Rebend test (32 to 40mm)- IS 1786: 2008) |
1500.0 |
|
| 9.2 (3) (Total Elongation at Maximum Force on gauge length of 5.65 Square Root of Crosss- Sectional Area, % - IS 1608 (Part 1): 2022.) |
- |
|
| 9.2 (2) (Elongation Percent on gauge length of 5.65 Square Root of Crosss- Sectional Area, % - IS 1608 (Part 1): 2022.) |
1000.0 |
|
| 4.2 (19) (Chemical composition of Micro alloying elements, % by mass.) |
4000.0 |
|
| 4.2 (1) (Carbon Equivalent (CE), , % by mass.) |
2000.0 |
|
|
| 3552 |
National Test House (SR), Chennai
| IS 1237 (2012) - Cement Concrete Flooring Tiles - Specification |
Cement Concrete Flooring Tiles - Specification |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 12.6 (Wet transverse strength-Annex F of IS 1237:2012) |
2000.0 |
|
| 12.5 (Water Absorption-Annex E of IS 1237:2012) |
1000.0 |
|
| 12.4 (Straightness-Annex D of IS 1237:2012) |
500.0 |
|
| 12.3 (Perpendicularity-Annex C of IS 1237:2012) |
500.0 |
|
| 12.2 (Flatness-Annex B of IS 1237:2012) |
500.0 |
|
| 10 (General Quality-IS 1237:2012) |
100.0 |
|
| 8.3 & Table2 (The thickness of Wearing Layer-IS 1237:2012) |
100.0 |
|
| 7, 8.2 & Table1 (Thickness & Tolerances-IS 1237:2012) |
100.0 |
|
| 7 & 8.1, Table1 (Dimensions & Tolerances-IS 1237:2012) |
200.0 |
|
| 12.7 (Resistance to wear-Annex G of IS 1237:2012) |
2500.0 |
|
| - (Density) |
1000.0 |
|
|
| 3553 |
National Test House (SR), Chennai
| IS 15658 (2021) - Concrete Paving Blocks - Specification ( First Revision ) |
Concrete Paving Blocks - Specification ( First Revision ) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 7.3, Table 3, Sl No (i) (Water Absorption-IS 15658:2021, Annex C) |
1000.0 |
|
| 7.3, Table 3, Sl No (ii) (Compressive Strength-IS 15658:2021, Annex D) |
4000.0 |
|
| 7.2, Table2 (Dimensions & Tolerances-IS 15658:2021, Annex B) |
3000.0 |
|
| 7.1 (General quality & Finish-IS 15658:2021) |
1000.0 |
|
| 7.3, Table 3, Sl No (iii) (Abrasion Resistance-(Dry condition)-IS 15658:2021, Annex E) |
4000.0 |
|
| 7.3, Table 3, Sl No (iii) (Abrasion Resistance-(Wet condition)-IS 15658:2021, Annex E) |
4000.0 |
|
| 7.3, , Table 3, Sl No (v) (Flexural strength-IS 15658:2021, Annex G) |
4000.0 |
|
|
| 3554 |
National Test House (SR), Chennai
| IS 12894 (2002) - Pulverized fuel ash - Lime bricks - Specification |
Pulverized fuel ash - Lime bricks - Specification |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 7.3 (Efforescence) |
1000.0 |
|
| 7.4 (Water Absorption) |
1000.0 |
|
| 7.1 (Crushing Strength) |
2000.0 |
|
| 5 (Dimensions) |
500.0 |
|
| 3 (General quality) |
500.0 |
|
| 7.2 (Drying Shrinkage) |
2000.0 |
|
|
| 3555 |
National Test House (NR), Ghaziabad
| IS 8110 (2019) - Water well screens and slotted pipes - Specification (Third Revision) |
Water well screens and slotted pipes - Specification (Third Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 8.3.6 (Visual) |
1000.0 |
|
| 5 (Chemical Analysis) |
5000.0 |
|
| 8.3.4 (Tensile load) |
5000.0 |
|
| 2 (Slotting arrangement) |
1000.0 |
|
| 7.2 (Diameter of screen) |
1000.0 |
|
| 8.1 (Thickness of pipe) |
1000.0 |
|
| 3.1 (Sulphur (% by mass)) |
700.0 |
|
| 3.1 (Phosphorous (% by mass)) |
700.0 |
|
|
| 3556 |
National Test House (SR), Chennai
| IS 1077 (1992) - Common burnt clay building bricks - Specification (Fifth Revision) |
Common burnt clay building bricks - Specification (Fifth Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 7.3 (Efflorescence IS 3495 (Part 3) : 2019) |
1000.0 |
|
| 7.2 (Water Absorption IS 3495 (Part 2) : 2019) |
1000.0 |
|
| 7.1 (Compressive Strength-IS 3495 (Part 1) : 2019) |
2000.0 |
|
| 6 (DIMENSIONS AND TOLERANCES-IS 1077 : 1992) |
500.0 |
|
| 5 (GENERAL QUALITY IS 1077 : 1992) |
500.0 |
|
|
| 3557 |
National Test House (SR), Chennai
| IS 16415 (2015) - Composite cement |
Composite cement |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 7 (Drying Shrinkage) |
1000.0 |
|
| 7 (Compressive strength,672±4 h) |
1000.0 |
|
| 7 (Compressive strength,168±2 h) |
1000.0 |
|
| 7 (Compressive strength,72±1 h) |
1000.0 |
|
| 7 (Setting time,Final) |
250.0 |
|
| 7 (Setting time Initial) |
250.0 |
|
| 7 (Soundness-autoclave method) |
1000.0 |
|
| 7 (Soundness-Lechatlier method) |
500.0 |
|
| 7 (Fineness) |
1000.0 |
|
|
| 3558 |
National Test House (SR), Chennai
| IS 455 (2015) - Portland slag cement - Specification |
Portland slag cement - Specification |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 7 (28 Days Compressive strength,672±4 h) |
1000.0 |
|
| 7 (7 Days Compressive strength,168±2 h) |
1000.0 |
|
| 7 (3 Days Compressive strength,72±1 h) |
1000.0 |
|
| 7 (Setting time,Final) |
250.0 |
|
| 7 (Setting time Initial) |
250.0 |
|
| 7 (Soundness-autoclave method) |
1000.0 |
|
| 7 (Soundness-Lechatlier method) |
500.0 |
|
| 7 (Fineness) |
1000.0 |
|
| 6 (Alkali content) |
1000.0 |
|
| 6 (Chloride content) |
700.0 |
|
| 6 (Loss on Ignition) |
700.0 |
|
| 6 (Sulphide Sulphur (S)) |
700.0 |
|
| 6 (Total Sulphur content calculated as sulphuric anhydride SO3) |
500.0 |
|
| 6 (Magnesia) |
700.0 |
|
| 6 (Insoluble residue) |
700.0 |
|
| 13 (Consistency of Cement) |
500.0 |
|
| custom (Compressive strength-24 ±2h) |
1000.0 |
|
|
| 3559 |
National Test House (NR), Ghaziabad
| IS 4270 (2001) - Steel tubes used for water wells specification (Third Revision) |
Steel tubes used for water wells specification (Third Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 14 (Workmanship) |
1000.0 |
|
| 5.2 (Sulphur) |
1250.0 |
|
| 9 (Outside diameter) |
3000.0 |
|
| 6.2 (Flattening) |
1000.0 |
|
| 6.1 (Tensile test) |
3000.0 |
|
| 7 (Weight in kg/m) |
1000.0 |
|
| 7 (Thickness) |
250.0 |
|
| 14 (Visual examination) |
1000.0 |
|
| 6.1 (Yield Strength) |
1000.0 |
|
| 6.1 (% Elongation) |
1000.0 |
|
| 5.2 (Phosphorus) |
1250.0 |
|
|
| 3560 |
National Test House (NR), Ghaziabad
| IS 1239 : Part 1 (2004) - Steel Tubes, Tubulars and Other Wrought Steel Fittings : Part 1 Steel Tubes (BI-LINGUAL) |
Steel Tubes, Tubulars and Other Wrought Steel Fittings : Part 1 Steel Tubes (BI-LINGUAL) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 12 (Galvanising (Mass of Zinc Coating)) |
2000.0 |
|
| 7 (Chemical Analysis ( As per Annexure)) |
3000.0 |
|
| 14.3 (Flattening Test on tube above 50 mm NB) |
1000.0 |
|
| 14.2 (Bend test on tube (upto and including 50 mm NB)) |
1000.0 |
|
| 8.1 (Mass per meter) |
1000.0 |
|
| 8 (Dimensions (Thickness), mm.) |
1000.0 |
|
| 14.1.1(a) (% Elongation) |
1000.0 |
|
| 14.1 (Tensile Strength) |
2000.0 |
|
| 15 (Workmanship) |
500.0 |
|
| 13 (Leak proof test) |
2500.0 |
|
| 12 (Uniformity of Coating) |
500.0 |
|
| 8 (Dimension (Outside diameter), mm.) |
1000.0 |
|
|
| 3561 |
National Test House (SR), Chennai
| IS 1489 (Part 1) (2015) - Portland pozzolana cement - Specification: Part 1 Fly Ash Based |
Portland pozzolana cement - Specification: Part 1 Fly Ash Based |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 7, Table 2, Sl No 1 (Fineness IS 4031(2):1999) |
1000.0 |
|
| 7, Table 2, Sl No 6 (Drying Shrinkage IS 4031(10):1988) |
1000.0 |
|
| 7, Table 2, Sl No 4c (28 Days Compressive strength, IS 4031(6):1988) |
1000.0 |
|
| 7, Table 2, Sl No 4b (7 Days Compressive strength, IS 4031(6):1988) |
1000.0 |
|
| 7, Table 2, Sl No 4a (3 Days Compressive strength, IS 4031(6):1988) |
1000.0 |
|
| 7, Table 2, Sl No 3b (Setting time-Final IS 4031(5):1988) |
250.0 |
|
| 7, Table 2, Sl No 3a (Setting time-Initial IS 4031(5):1988) |
250.0 |
|
| 7, Table 2, Sl No 2b (Soundness-autoclave method IS 4031(3):1988) |
1000.0 |
|
| 7, Table 2, Sl No 2a (Soundness-Lechatlier method IS 4031(3):1988) |
500.0 |
|
| 6, Table 1, Sl No 6 (Alkali content IS 4032:1985) |
2000.0 |
|
| 6, Table 1, Sl No 5 (Chloride content, IS 4032:1985) |
800.0 |
|
| 6, Table 1, Sl No 4 (Loss on ignition IS 4032:1985) |
800.0 |
|
| 6, Table 1, Sl No 3 (Total Sulphur content IS 4032:1985) |
800.0 |
|
| 6, Table 1, Sl No 2 (Magnesia IS 4032:1985) |
600.0 |
|
| 6, Table 1, Sl No 1 (Insoluble residue, IS 4032:1985) |
1000.0 |
|
| 13 (Consistency of Cement) |
500.0 |
|
| 7 (Compressive strength-24 +/- 1 h) |
1000.0 |
|
| Custom (Fineness of Cement by Wet Sieving [as per IS 4031 (Part 15): 1991]) |
500.0 |
|
|
| 3562 |
National Test House (SR), Chennai
| IS 280 (2006) - Mild steel wire for general engineering purposes (Fourth Revision) |
Mild steel wire for general engineering purposes (Fourth Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 9.2 (Wrapping Test) |
1000.0 |
|
| 9.1 (Tensile Strength) |
3000.0 |
|
|
| 3563 |
National Test House (SR), Chennai
| IS 277 (2018) - Galvanized steel strips and sheets (Plain And Corrugated) - Specification (Seventh Revision) |
Galvanized steel strips and sheets (Plain And Corrugated) - Specification (Seventh Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 14 (Total coated thickness, mm) |
1000.0 |
|
| 8.1 (Erischen cupping test) |
1000.0 |
|
| 8.2 (Bend Test) |
1000.0 |
|
| 8.1 (Percentage Elongation, %) |
1000.0 |
|
| 8.1 (Yield Strength, MPa) |
1000.0 |
|
| 8.1 (Tensile strength, MPa) |
1000.0 |
|
| 8.1 (Mass of Zn coating) |
2000.0 |
|
| 5.1 (Carbon) |
500.0 |
|
| 5.1 (Manganese) |
500.0 |
|
| 5.1 (Sulphur) |
500.0 |
|
| 5.1 (Phosphorus) |
500.0 |
|
| 9 (Surface roughness) |
1000.0 |
|
| 14 (Thickness (As received condition), mm) |
1000.0 |
|
| TDS-1 (Base Metal Thickness (As per test request), mm) |
1000.0 |
|
| 5.1 (Aluminium) |
500.0 |
|
| 5.1 (Silicon) |
500.0 |
|
| TDS-2 (Dimension, mm) |
2000.0 |
|
|
| 3564 |
National Test House (SR), Chennai
| IS 278 (2009) - Galvanized steel barbed wire for fencing - Specification (Fourth Revision) |
Galvanized steel barbed wire for fencing - Specification (Fourth Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 12.1 (Breaking Load of Completed Barbed Wire) |
1000.0 |
|
| 12.1 (Tensile Strength of Line Wire) |
1000.0 |
|
| 12.3 (Ductility) |
1000.0 |
|
|
| 3565 |
National Test House (WR), Mumbai
| IS 814:2004 - Covered electrodes for manual metal arc welding of carbon and carbon manganese steel - Specification (Sixth Revision) |
Covered electrodes for manual metal arc welding of carbon and carbon manganese steel - Specification (Sixth Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 9.6 (Radiographic Test-IS 1182) |
1000.0 |
|
| 9.4 (Increased Metal Recovery Test-IS 13043) |
3000.0 |
|
| 9.5 (Diffusible Hydrogen Evaluation Test-IS 11802) |
5000.0 |
|
| 9.2 (Butt Weld Bend Test -IS 1599) |
8000.0 |
|
| 9.1.3 (Impact Strength-Annex F) |
3000.0 |
|
| 9.1.2 (Percentage Elongation on Gauge Length-Annex F) |
1000.0 |
|
| 9.1.2 (Yield Stress -Annex F) |
1000.0 |
|
| 9.1.2 (Ultimate Tensile Strength -Annex F) |
1000.0 |
|
| 9.1.1 (Preparation of Weld assembly) |
4000.0 |
|
| B7 (Coating Ratio) |
500.0 |
|
| 7.4 (Defects of Core Wire and Coverings) |
250.0 |
|
| 7.3 (Concentricity of Flux Covering With Core Wire) |
250.0 |
|
| 7.2.2 (Arc striking End) |
500.0 |
|
| 7.2.1 (Contact End) |
500.0 |
|
| 7.1.2 (Length of Electrode) |
500.0 |
|
| 7.1.1 (Diameter of Core Wire) |
500.0 |
|
|
| 3566 |
National Test House (SR), Chennai
| IS 9537 : Part 2 (1981) - Specification for conduits for electrical installations: Part 2 rigid steel conduits |
Specification for conduits for electrical installations: Part 2 rigid steel conduits |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 9.2 (Bend Test) |
1000.0 |
|
| 7 (Wall thickness of 63 mm nominal size) |
500.0 |
|
| 9.2 (Bending Test (With Seam on the Outside of flank)) |
500.0 |
|
| 9.2 (Bending Test (With Seam on the flank)) |
500.0 |
|
| 13 (External Influence Test (With Seam on the Outside of the Bend)) |
1000.0 |
|
| 13 (External Influence Test (With Seam on the flank)) |
1000.0 |
|
| 7 (Wall thickness) |
500.0 |
|
| 7 (Outside Diameter) |
500.0 |
|
| 7 (Outside Diameter of 50 mm nominal size) |
500.0 |
|
| 7 (Outside Diameter of 40 mm nominal size) |
500.0 |
|
| 7 (Outside Diameter of 32 mm nominal size) |
500.0 |
|
| 7 (Outside Diameter of 25 mm nominal size) |
500.0 |
|
| 7 (Outside Diameter of 20 mm nominal size) |
500.0 |
|
| 7 (Outside Diameter of 16 mm nominal size) |
500.0 |
|
| 7.2 (Checking the Minimum outside diameter.) |
750.0 |
|
| 7.2 (Checking the Maximum outside diameter) |
750.0 |
|
| 9.2 (Bending Test (With Seam on the Outside of flank)) |
500.0 |
|
| 9.2 (Bending Test (With Seam on the flank)) |
500.0 |
|
| 13 (External Influence Test (With Seam on the flank)) |
1000.0 |
|
| 13 (External Influence Test (With Seam on the Outside of the Bend)) |
1000.0 |
|
| 9.3 (Compression Test) |
3000.0 |
|
| 0.1 (Mass of Zn Coating) |
2000.0 |
|
| 0.3 (Uniformity of Zn Coating) |
1000.0 |
|
|
| 3567 |
National Test House (SR), Chennai
| IS 2062 (2011) - Hot rolled medium and high tensile structural steel - Specification (Seventh Revision) |
Hot rolled medium and high tensile structural steel - Specification (Seventh Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 15 (Dimensions) |
1000.0 |
|
| 12 (Impact Test (For Specified Quality Grade)) |
5000.0 |
|
| 11 (Bend Test - IS 1599: 2019.) |
1500.0 |
|
| 10 (% Elongation - IS 1608 (Part 1): 2022.) |
1000.0 |
|
| 10 (Yield Stress - - IS 1608 (Part 1): 2022.) |
1000.0 |
|
| 10 (Tensile Strength - IS 1608 (Part 1): 2022) |
1000.0 |
|
| 8.2 (Carbon Equivalent, %) |
500.0 |
|
| 8.2 (Silicon) |
500.0 |
|
| 8.2 (Manganese) |
500.0 |
|
| 8.2 (Phosphorus) |
500.0 |
|
| 8.2 (Sulphur) |
500.0 |
|
| 8.2 (Carbon) |
500.0 |
|
| 0 (Coating Thickness) |
2000.0 |
|
| 0 (Mass of Zinc Coating) |
2000.0 |
|
| 8 (Chemical Analysis) |
2500.0 |
|
| 8 (Chemical Analysis with micro-alloys) |
5000.0 |
|
| 8.2 (Carbon Equivalent (CE), %.) |
500.0 |
|
| 4 (Diameter (IS 1732), mm) |
1000.0 |
|
| 4 (Mass per metre (IS 1732), kg) |
1000.0 |
|
|
| 3568 |
National Test House (SR), Chennai
| IS 4985 (2000) - Unplasticized pvc pipes for potable water supplies - Specification (Third Revision) |
Unplasticized pvc pipes for potable water supplies - Specification (Third Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 11.2 (Resistance to External Blows) |
2000.0 |
|
| 11.1 (Hydrostatic Characteristics) |
5000.0 |
|
| 10.6 (Density) |
2000.0 |
|
| 10.5 (Vicat Softening Temperature) |
1500.0 |
|
| 10.4 (Reversion Test) |
2000.0 |
|
| 10.2 (Opacity) |
2000.0 |
|
| 7.2 (Dimension of Socket) |
1000.0 |
|
| 7.1 (Dimension of Pipe) |
1000.0 |
|
| 10.1 (Visual Appearance) |
1000.0 |
|
| 9.1 (Pipe End) |
1000.0 |
|
|
| 3569 |
National Test House (ER), Kolkata
| IS 3576 (2010) - Spices and condiments - Turmeric, whole and ground - Specification (Third Revision) |
Spices and condiments - Turmeric, whole and ground - Specification (Third Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 4.5 (xi) (Cadmium) |
500.0 |
|
| 4.5 (x) (Zinc) |
500.0 |
|
| 4.5 (viii) (Copper) |
500.0 |
|
| 4.5 (vii) (lead) |
500.0 |
|
| 4.5 (vi) (presence of chromate) |
500.0 |
|
| 4.5 (v) (starch) |
500.0 |
|
| 4.5 (iii) (Dilute HCl insoluble ash) |
500.0 |
|
| 4.5 (ii) (Total ash) |
500.0 |
|
| 4.5 (i) (Moisture) |
500.0 |
|
| 4.6 (Fineness) |
500.0 |
|
| 4.2 (Freedom from moulds, insects etc) |
500.0 |
|
| 4.1 (Odour and flavour) |
500.0 |
|
|
| 3570 |
National Test House (ER), Kolkata
| IS 2443 (2008) - Spices and condiments - Coriander, whole and ground - Specification (Third Revision) |
Spices and condiments - Coriander, whole and ground - Specification (Third Revision) |
- View breakup
-
| Clause No. |
Testing Charges (Excl. Of Taxes) |
NABL |
| 3.2(iii) (Acid insoluble ash, powder) |
1200.0 |
|
| 3.2(ii) (Total ash, powder) |
1200.0 |
|
| 3.2(i) (Moisture, powder) |
1200.0 |
|
| 3.1.3 (Freedom from moulds, insects etc, whole) |
1200.0 |
|
| 3.1.2 (Taste and flavour, whole) |
1200.0 |
|
| 3.1.1 (Description, whole) |
1200.0 |
|
| 3.2.4 (Fineness) |
1200.0 |
|
| 3.2(iv) (Volatile oil, powder) |
1200.0 |
|
| 3.2(v) (Salmonella, powder) |
1200.0 |
|
|